- Always dry your material per the time and temperature specified in the matrix. Wet material can cause weak layer bonding, holes in your prints, and bad print aesthetics.
- Do not touch the outside of the printer when fully heated except for handles. Do not touch anything inside the printer while printing.
- Use the provided work gloves and eye protection to avoid burns or injuries when working with the printer.
- Don't open the chamber immediately after a print and attempt to remove the part:
- Instead, let the build plate naturally cool down to room temperature, and the prints will pop off on their own.
- Attempting to force a print off the plate when hot can damage your print, damage the print surface, and throw out the bed calibration.
Use this cheat sheet to quickly reference material specifications.
|
PLA |
ABS |
ASA |
TPU |
PC |
CF-PEI |
CF-PEEK |
CF-PEKK-C |
PEI-9085 |
PEEK |
PEKK-C |
PSU |
| Nozzle Temp |
215C |
240C |
250C |
225C |
290C |
385C |
460C |
390C |
360C |
450C |
380C |
370C |
| Bed Temp |
60C |
110C |
105C |
75C |
120C |
180C |
190C |
190C |
190C |
190C |
190C |
200C |
| Chamber Temp |
N/A |
65C |
65C |
N/A |
72C |
90C |
95C |
90C |
90C |
90C |
90C |
90C |
| Print Speed |
50-100 |
50-100 |
50-100 |
20-30 |
50-70 |
20-60 |
25-50 |
30-70 |
50-80 |
25-50 |
30-70 |
30-60 |
| Cooling Fan |
100% |
75% |
75% |
100% |
0% |
0% |
0% |
0% |
0% |
0% |
0% |
0% |
| Drying Time |
50C/4hr |
70C/6hr |
70C/6hr |
60C/12hr |
80C/12hr |
125C/12hr |
150C/12hr |
150C/12hr |
125C/12hr |
150C/12hr |
135C/12hr |
125C/12hr |
| Annealing |
N/A |
N/A |
N/A |
N/A |
N/A |
Optional |
Required |
Required |
Optional |
Required |
Required |
Optional |